Originally Posted by
grizzman
I have one nitrided bolt carrier, and it's showing some wear on the rails and inside the gas cylinder after around 250 rounds fired. I presume the Noveske is chrome lined.
I think I'll personally stick with phosphated and chromed for now.
That was my thoughts exactly. I am not 100% sold on this whole nitrate coating yet. Chrome lined has served me very well for many years and I have to see a huge difference before I switch.
In no way do I make any money from anyone related to the firearms industry.
"I have never heard anyone say after a firefight that I wish that I had not taken so much ammo.", ME
"Texas can make it without the United States, but the United States can't make it without Texas !", General Sam Houston